Increase of susceptibility to the initiation of ammonium nitrate TNT containing mixtures
Abstract
Obtained by coarsely dispersed granulites with a diameter of granules of 0.5-1.0, with percentages of ammonium nitrate, 80%, TNT 20%. 79 % 21%. Reliably detonate of detonator capsule CD-8A.
References
1. Дубнов Л.В. Промышленные взрывчатые вещества. Москва. Недра. 1992г., с. 237-236.
2. Друкованный М. Ф., Кукиб Б. Н., Куц В. С. Буровзрывные работы на карьерах. Москва. Недра. 1990 г.
This work is licensed under a Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International License.
Authors retain copyright and grant the journal right of first publication with the work simultaneously licensed under a Creative Commons Attribution License (CC BY-NC-ND 4.0) that allows others to share the work with an acknowledgement of the work's authorship and initial publication in this journal.